DIAL GAUGE BASE COMPOSED BY:
SPRING + PIN + DISC + BASE UPR + BASE LWR
HEAT TREATMENT OF CARBURIZING AND HARDENING WITH A HARDNESS OF 58 – 60 HRC AND DEPTH 0.8MM TO 1.0MM.
SURFACE TREATMENT OF BLACK OXIDATION ON ALL PARTS.
OBS.: SPRING IN HARDENED SPRING STEEL.
THE MATERIAL IS SAE 8620.